Reduced Graphene Oxide rGO
Obtained by reducing Graphene Oxide (GO).
Specification
- Form: Powder
- Reduction method: Chemically reduced
- Sheet dimension: Variable
- Color: Black
- Odor: Odorless
- Solubility: Insoluble
- Dispersability: It can be dispersed at low concentrations (<0.1mg/mL) in NMP, DMSO, DMF
- Humidity (Karl Fisher, TGA): 3.7 - 4.2%
- Electrical conductivity: 666,7 S/m (*)
- BET surface area: 422.69 – 499.85 m2/g
- Density: 1.91 g/cm3
- (*) Measured in a 20nm film thickness
- Quality control: Elemental Analysis
Elemental Analysis
- C (%): 77 – 87%
- H (%): 0 – 1%
- N (%): 0 – 1%
- S (%): 0
- (%): 13 – 22%